Deformation of Different Nickel-Titanium Rotary Systems after Repeated Use [An In Vitro Study]

Mohamed Nabeel Ahmed Hashem;

Abstract


The resistance to deformation and/or fracture of four different nickel-titanium rotary systems was evaluated. The tested systems were: Group (1): ProTaper (Dentsply Maillefer, Ballaigues, Switzerland), Group (2): RaCe (FKG Dentaire, La-Chaux-de-Fonds, Swi


Other data

Title Deformation of Different Nickel-Titanium Rotary Systems after Repeated Use [An In Vitro Study]
Other Titles تشوه مبارد أنظمة نيكل - تيتانيوم الدوارة عقب تكرار الاستخدام ]دراسة معملية [
Authors Mohamed Nabeel Ahmed Hashem
Keywords Deformation of Different Nickel-Titanium Rotary Systems after Repeated Use [An In Vitro Study]
Issue Date 2011
Description 
The resistance to deformation and/or fracture of four different nickel-titanium rotary systems was evaluated. The tested systems were: Group (1): ProTaper (Dentsply Maillefer, Ballaigues, Switzerland), Group (2): RaCe (FKG Dentaire, La-Chaux-de-Fonds, Swi

Attached Files

File SizeFormat
100370Binder1.pdf3.38 MBAdobe PDFView/Open
Recommend this item

Similar Items from Core Recommender Database

Google ScholarTM

Check

views 2 in Shams Scholar


Items in Ain Shams Scholar are protected by copyright, with all rights reserved, unless otherwise indicated.