Ultramorphology and Bond Strength of Self-Etching Bonding Agents to Demineralized and Remineralized Enamel
Hossam El-Hussien Mohamed El-Zuhery;
Abstract
The improvement of adhesion of dental resins to human enamel with the use of the acid-etching procedure is considered the basis of modern cosmetic and conservative restorative dentistry (Buonocore, 1955).
Traditionally, enamel etching has been made wi
Traditionally, enamel etching has been made wi
Other data
| Title | Ultramorphology and Bond Strength of Self-Etching Bonding Agents to Demineralized and Remineralized Enamel | Authors | Hossam El-Hussien Mohamed El-Zuhery | Keywords | Ultramorphology and Bond Strength of Self-Etching Bonding Agents to Demineralized and Remineralized Enamel | Issue Date | 2009 | Description | The improvement of adhesion of dental resins to human enamel with the use of the acid-etching procedure is considered the basis of modern cosmetic and conservative restorative dentistry (Buonocore, 1955). Traditionally, enamel etching has been made wi |
Attached Files
| File | Size | Format | |
|---|---|---|---|
| 74133r602.pdf | 88.38 kB | Adobe PDF | View/Open |
Similar Items from Core Recommender Database
Items in Ain Shams Scholar are protected by copyright, with all rights reserved, unless otherwise indicated.