Plastic Behavior Due to Ge Precipitation in Al-based Alloys

Jacklein Anwar Fawzy Riad;

Abstract


The present thesis mainly covers,

1. The effect of both aging temperatures (Ta = 323, 348, 373, 398, 423, 448, 473, 498, 523, 548 and 573 K) and aging times (ta = 0.25, 0.5, 1, 2, 4 and 6 hr) on the stress- strain behavior of Al- 4 wt % Ge alloy wire s


Other data

Title Plastic Behavior Due to Ge Precipitation in Al-based Alloys
Other Titles السلوك اللدن نتيجة ترسيب الجرمانيوم في سبائك قاعدتها الألومنيوم
Authors Jacklein Anwar Fawzy Riad
Keywords Plastic Behavior Due to Ge Precipitation in Al-based Alloys
Issue Date 2013
Description 
The present thesis mainly covers,

1. The effect of both aging temperatures (Ta = 323, 348, 373, 398, 423, 448, 473, 498, 523, 548 and 573 K) and aging times (ta = 0.25, 0.5, 1, 2, 4 and 6 hr) on the stress- strain behavior of Al- 4 wt % Ge alloy wire s

Attached Files

File SizeFormat
120724g1302.pdf200.62 kBAdobe PDFView/Open
Recommend this item

Similar Items from Core Recommender Database

Google ScholarTM

Check

views 10 in Shams Scholar


Items in Ain Shams Scholar are protected by copyright, with all rights reserved, unless otherwise indicated.